Answers are grounded in this paper and cite their sources.
High temperatures can cause severe damage to the load-bearing capacity and internal integrity of concrete. The residual performance of 1:2:4 concrete with carbon fibers based on polyacrylonitrile at 0%, 1% and 2% of the cement mass was investigated in this work. 36 100-mm cube specimens were cured for 28 days and exposed for 24 h to nominal temperatures of 25, 250, 500 and 750 °C. Residual compressive strength and direct-transmission ultrasonic pulse velocity (UPV) were tested after cooling. Differences among the 12 treatment groups were estimated using one-way analysis of variance (ANOVA) and Tukey’s honestly significant difference (HSD) test. The compressive strength decreased with the increase in temperature, while the residual strength increased with the addition of carbon fiber. The control, 1% and 2% fiber mixes showed strengths of 7, 10 and 11 MPa, respectively, at 500 °C with 40.0%, 55.6% and 55.0% retention of the ambient temperature strengths. The 2% fiber mix was 57.1% stronger than the control. The residual strength at 750 °C was 5 MPa (25.0% retention), which is double the control strength of 2.5 MPa (14.3% retention). Control-mixture UPV dropped from 4.54 km/s (25 °C) to 3.30 km/s (750 °C). The velocity of the 500 °C fiber mixtures was 4.10 km/s, and for the control, 3.80 km/s. The ANOVA analysis showed that the treatment groups were significantly different from each other (F = 1,114.96, p < 0.0001). The highest residual strength of the three conditions tested was observed for the 2 % carbon fiber.
No takes yet. Share an insight, caveat, or question.
Hussein et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: