Answers are grounded in this paper and cite their sources.
In this work, p-type monocrystalline silicon was compared after phosphorus diffusion from two sources: commercial POCl 3 (Sidp) and a spin-on solution S extracted from purified Tunisian natural phosphate by nitric-acid dissolution and filtration. Solution S was applied on planar silicon (SidS) and on porous silicon (SipdS) formed by HF/HNO 3 vapour etching for 30 s, the etching time being selected by atomic force microscopy and reflectance. After diffusion at 925°C for 45 min, hot-probe measurements showed n+ conduction in nearly all measurements on the three samples, and the sheet resistance of the doped layers was above that of the undoped control (107.23 Ω/sq). Dark I–V analysis, although strongly non-ideal, and effective minority-carrier lifetime measurements gave the same ranking: the best sample was porous silicon diffused with solution S (SipdS), which showed the lowest saturation current (0.92 µA against 10.34 µA for POCl 3 ), the lowest series resistance, the highest shunt resistance and the longest lifetime (92 µs against 31 µs). A phosphorus source derived from Tunisian phosphate therefore gives samples at least comparable to, and in this comparison better than, the POCl 3 reference; dopant profiles, passivated lifetime and device data are needed to confirm this.
No takes yet. Share an insight, caveat, or question.
Daik et al. (2026) studied this question.
Synapse has enriched 8 closely related papers on similar clinical questions. Consider them for comparative context: