This work focuses on studying processing, microstructure formation, and mechanical behaviour of aluminium 6061 matrix composites, reinforced with SiC particles by stir casting and heat treatment methods, i.e. solutioning, quenching, and artificial ageing. To conduct the current study, composite samples were manufactured using varying weight ratios of SiC (4% weight, 8% weight and 12% weight) and the control specimen was made by using the matrix alloy. It was noted that the reinforcement in solidification with SiC increased the refinement of the grain itself due to its pinning effect that limited the mobility of the grain boundaries. In all the compositions, 12% SiC sample had a highest tensile strength of 125.26 Mpa against 90 Mpa without reinforcing alloy in 6061 aluminium. This hardening was, however, coupled with ductility loss, with elongation decreasing from 12 % in the base alloy to 5.98 % in the 12 % SiC composite. Charpy impact tests revealed that the level of energy absorption capacity increased to 3 J at 12% SiC composite whereas at the unreinforced alloy, a transfer of stress to hard SiC particles increased to 1 J. Hardness testing also gave significant improvement with the highest Rockwell hardness of 81 HRC with the 4% SiC composite. The high reinforcement (12%)-level led to slight hardness and elongation reductions, which was because of the agglomeration of particles and interfacial flaws, which meets SDG goal 9 Progress in the creation and development of complex composite substrates.
No takes yet. Share an insight, caveat, or question.
Kumar et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: