Answers are grounded in this paper and cite their sources.
Objectives To evaluate the effect of blood and blood‐saliva contamination on the shear bond strength (SBS) of All‐Bond Universal adhesive to Mineral Trioxide Aggregate (MTA) and to compare the effectiveness of different cleaning protocols in restoring SBS. Materials and Methods A total of 132 cylindrical MTA‐Angelus specimens were fabricated, allowed to set for 72 h, acid‐etched for 5 s, and randomly divided into 11 groups (n = 12). G1 served as the uncontaminated control. Groups G2–G11 comprised two contamination conditions (blood and blood–saliva) and five treatment protocols (no treatment, rinsing, phosphoric acid, gallic acid, and Katana Cleaner). G2–G6 comprised blood‐contaminated specimens subjected to no treatment, rinsing only, rinsing followed by phosphoric acid, rinsing followed by gallic acid, or Katana Cleaner, respectively. G7–G11 comprised blood‐saliva‐contaminated specimens treated using the same protocols in the same order. The specimens were bonded with All‐Bond Universal and everX Flow. SBS was measured. Data were analyzed using Welch's ANOVA and Games–Howell post hoc test (α = 0.05). Fracture modes and surface micromorphology were evaluated. Results All decontamination protocols significantly increased SBS compared with the corresponding untreated contaminated groups (all p < 0.001). Phosphoric acid and gallic acid showed significantly higher SBS values than the rinsing and Katana Cleaner groups in two conditions (all p < 0.001), with no significant difference between the two acids. In both blood and blood‐saliva contamination, SBS after phosphoric acid (9.50 ± 1.49 and 9.10 ± 1.46, respectively) and gallic acid treatment (10.35 ± 1.59 and 9.47 ± 1.72, respectively) was comparable to that of uncontaminated control group (8.67 ± 0.98). Conclusion According to this in vitro finding, gallic acid and phosphoric acid etching with prior water rinsing under blood and blood‐saliva contamination may be an effective approach for achieving high resin–MTA bond strength in contaminated conditions. Katana Cleaner with no prior rinsing exhibited lower effectiveness than acidic agents.
No takes yet. Share an insight, caveat, or question.
Shafıei et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: