Low‐temperature and high‐rate charging imposes limitations on graphite anodes, driving local potentials below 0 V vs. Li/Li + and triggering lithium plating, which accelerates capacity fade and compromises safety. Conventional voltage monitoring is insensitive to the mechanical signatures of lithium deposition. Here, we investigate expansion pressure response of 32 Ah prismatic LiFePO 4 /graphite cells under various charging conditions and introduce a differential metric, d P /d Q (pressure change per unit capacity), to amplify the mechanical footprint of plating. Results show that d P /d Q surges sharply during the late stage of low‐temperature charging, far above the ambient‐temperature baseline, enabling identification of graphite‐anode plating onset. We establish a detection threshold based on the maximum d P /d Q during normal intercalation and propose a temperature‐compensated variant to minimize false alarms under varying operating temperatures. To evaluate graphite‐anode plating severity, cells with controlled plating degrees are prepared via low‐temperature cycling; five peak‐shape features extracted from pressure curves exhibit monotonic trends with capacity loss, providing indicators for relative severity assessment. Plated cells show gradual capacity recovery over subsequent cycles, revealing a reversible window for timely intervention before irreversible loss dominates. This mechanical‐sensing framework offers a practical, non‐invasive approach for relative plating severity assessment under controlled single‐cell conditions.
No takes yet. Share an insight, caveat, or question.
Xiong et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: