Addressing safety issues such as internal short circuits and thermal runaway caused by crack-dendrite co-evolution induced by defects in solid state lithium-metal batteries (SSLMBs), an electro-chemo-thermal-mechanical coupled phase-field model is developed. Impacts of initial crack geometric characteristics, crack number, and intercell temperature gradients on crack propagation and dendrite growth behavior are systematically investigated to reveal the underlying regulatory mechanisms. Results show that effects of initial crack shape on crack propagation and dendrite growth depend on crack size. Among the configurations investigated, the two-crack configuration exhibits the smallest maximum growth distance and pronounced outward crack deflection. At 200 s, its combined crack and dendrite area is approximately 32% smaller than that of the single-crack configuration, while its maximum crack propagation distance decreases from 225.4 to 69.4 μm, a reduction of approximately 69.2%. Interactions between the stress fields of adjacent cracks contribute to this suppression and crack deflection, reducing the risk of short circuits. Temperature heterogeneity across the cell also alters crack propagation paths and dendrite growth patterns. Under large intercell temperature heterogeneities, pronounced crack deflection is accompanied by suppressed dendrite growth. The findings of this study provide a rational guidance for SE/anode interface engineering, thermal management strategy developing, thus to regulate directional crack-dendrite co-evolution and upgrade cycle life for SSLMBs.
No takes yet. Share an insight, caveat, or question.
Pei et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: