Answers are grounded in this paper and cite their sources.
N-type Bi2Te2.5Se0.5 alloys exhibit a severe donor-like effect during powder metallurgy fabrication, which gives rise to excessively carrier concentration and degraded near-room-temperature thermoelectric performance. Suppressing the donor-like effect while preserving high carrier mobility remains a major bottleneck. Herein, Ag2Te/Bi2Te2.5Se0.5 composites are fabricated via mechanical alloying and spark plasma sintering. Owing to interfacial diffusion between superionic Ag2Te and the Bi2Te2.5Se0.5 matrix, some Ag atoms occupy dual crystallographic sites by substituting at Bi lattice sites and intercalating into van der Waals gaps, which suppresses the donor-like effect and lowers the carrier concentration. At the phase-transition point of Ag2Te at ~420 K, reversal of the built-in electric field at the heterogeneous-interface enables enhanced carrier mobility below the transition temperature. Total thermal conductivity reduction originates from both decreased carrier thermal conductivity and suppressed lattice thermal conductivity induced by multiscale defects. The AT04 composite delivers a peak ZT of 1.23 at 410 K. At room temperature, the ZT of AT04 is 0.98, corresponding to an 80% enhancement relative to pristine Bi2Te2.5Se0.5 (ZT = 0.54). This work provides new mechanistic insights and an effective strategy for utilizing phase-transition-tunable hetero-interfaces to boost the thermoelectric performance of Bi2Te3 and other thermoelectric materials.
No takes yet. Share an insight, caveat, or question.
Ma et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: