Answers are grounded in this paper and cite their sources.
Aggressive ions attack reinforcing steel in saline soil environments, and once the passive film on HRB400 steel destabilizes, localized corrosion spreads rapidly. Most studies vary the concentration of a single ion; how the SO42−/Cl− ratio governs film breakdown remains unclear. HRB400 specimens were immersed in simulated concrete pore solution and dosed stepwise with solid salts. Single-chloride and single-sulfate systems were used as controls; combined systems had SO42−/Cl− ratios of 1, 3 and 5. OCP, LPR and EIS were recorded at every step, with SEM/EDS on selected specimens. With chloride alone the passive film destabilized at 0.03–0.04 mol/L Cl− (mean OCP); with sulfate alone the corrosion current density fell up to 0.05 mol/L SO42−, and the destabilization occurred only at 0.11–0.12 mol/L. Raising the ratio shifted destabilization to 0.05–0.06, 0.06–0.07 and 0.11–0.12 mol/L, about 1.57, 1.86 and 3.29 times the chloride-only value, and at 0.10 mol/L Cl− (240 h) mean icorr fell from 7.71 to 5.98, 3.19 and 1.26 μA/cm2 (n = 3). Na+ and K+ were not varied independently; the concentrations refer to the pore solution. Sulfate therefore delays rather than prevents destabilization, and the ratio, not the chloride concentration alone, determines when the film fails.
No takes yet. Share an insight, caveat, or question.
Liu et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: