Answers are grounded in this paper and cite their sources.
Fatigue resistance governs the failure of many engineering components and hydrogen exposure may reduce fatigue life through hydrogen embrittlement (HE). The aim of this study is to examine the influence of cyclic predeformation on the HE behavior of AISI 321 stainless steel under low‐cycle fatigue (LCF). Cylindrical specimens are predeformed for 100 cycles at strain amplitudes of 0.3%–0.6%, followed by thermal charging in gaseous hydrogen at 350 °C and 5.1 MPa for 28 days. To separate hydrogen effects from thermal exposure, precycled reference specimens received an identical thermal treatment in air. Subsequent LCF tests are performed at ambient temperature under a constant strain rate. At strain amplitude of 0.6%, the precycled microstructure showed slip/shear bands, deformation twins, dislocation cells, with only limited deformation‐induced martensite. Hydrogen precharging reduced fatigue life and decreased the fatigue ductility coefficient from 0.0722 to 0.0577, whereas precycling did not affect the fatigue life. Fractographic examination of the hydrogen precharged test bars showed quasicleavage fracture with regions of fatigue striations, independent of prior precycling. The underlying HE mechanisms associated with these findings are discussed. The results suggest that, under the present test conditions, precycling is not required for the assessment of HE.
No takes yet. Share an insight, caveat, or question.
Anilkumar et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: