The precise characterization of microvoids within mesophase pitch-based carbon fibers (MPCF) is neccessary in order to enhance their thermal conductivity but remains a significant challenge. In this paper, the microvoid structure of three commercial MPCF is for the first time quantitatively characterized using field-emission scanning electron microscopy, small-angle X-ray scattering and high-resolution transmission electron microscopy. The results reveal that from XN-90 to K13D2U to K1100, the average longitudinal extension of the voids decreases from 656 ± 27 nm to 551 ± 11 nm. Concurrently, the orientation factor increases from 0.9743 ± 0.0016 to 0.9944 ± 0.0014, indicating progressively higher pore alignment. Radial pore size distribution analysis shows that the average microvoid size is largest for K1100. The pores in XN-90 and K13D2U are primarily small to medium-sized (<200 nm), whereas K1100 exhibits the highest proportion in the 200–300 nm range and a notable presence of large pores (>300 nm). The synergistic optimization of axial pore length, orientation and radial size distribution is associated with enhanced thermal conductivity. Additionally, transmission electron microscopy is employed to measure pores in both axial and radial directions. This multi-faceted characterization approach offers a refined methodology for accurately determining microscopic pore information in MPCF, offering a clear pathway for material optimization toward next-generation high-thermal-conductivity MPCF.
No takes yet. Share an insight, caveat, or question.
Wang et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: