Answers are grounded in this paper and cite their sources.
This paper reports the study of how isothermal cooling—a physical metallurgical processing technique—affects interstitial iron concentration and minority carrier lifetime in p-type Czochralski silicon for photovoltaic applications. The experimental results demonstrate that thermal-induced degradation of minority carrier lifetime occurs in p-type Czochralski wafers subjected to isothermal holding across a range of temperatures following heating at 900 °C. Under identical heating conditions, varying the subsequent isothermal holding temperature reveals a clear extremum: interstitial iron concentration decreases monotonically as temperature rises from 450 °C up to 650 °C, reaching its minimum at 650 °C; conversely, minority carrier lifetime increases with temperature in this regime and peaks at 650 °C. Above 650 °C, interstitial iron concentration increases and minority carrier lifetime declines. Thus, isothermal holding at 650 °C optimizes iron precipitation—minimizing interstitial iron concentration while maximizing minority carrier life-time. Holding time-dependent experiments at 650 °C (holding durations: 0, 30, 60, 120, 180, and 240 min) further show that interstitial iron concentration decreases monotonically with increasing holding time, accompanied by a corresponding monotonic increase in minority carrier lifetime.
No takes yet. Share an insight, caveat, or question.
Zhou et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: