Dissimilar weld joints between P92 steel and AISI 304H austenitic stainless steel are widely employed in the high-temperature components of supercritical thermal power plants, where both strength and long-term reliability are important. In the present investigation, 8 mm thick P92 steel–AISI 304H joints were fabricated using the Activated Flux Tungsten Inert Gas (A-TIG) welding process, and their mechanical response was examined at elevated temperatures of 500°C, 550°C, and 600°C. Tensile testing revealed that the welded joint retained higher strength than the individual base metals over the entire temperature range, fracture consistently occurred within the P92 steel. This behaviour is attributed to temperature-induced softening arising from carbide coarsening and the reduction of solid-solution strengthening. With increasing temperature, a gradual decrease in tensile strength and ductility was observed. Deformation was found to initiate on the more ductile AISI 304H side before transferring to the martensitic P92 region. Fractographic analysis using FE-SEM confirmed ductile fracture through micro-void nucleation and coalescence. Impact toughness improved significantly at elevated temperatures compared to room-temperature values. Creep-rupture life was estimated from a Larson–Miller curve for weldments, at 100–140 MPa. Creep–rupture life exceeded 10 6 h at 500°C and 550°C, whereas at 600°C it ranged from 2.7 × 10 4 to 2.0 × 10 5 h. High-temperature tensile behaviour combined with a Larson-Miller estimate thus gives a first approximation of creep-rupture life in this joint when long-term creep data are unavailable.
No takes yet. Share an insight, caveat, or question.
Sharma et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: