Although Tb-based grain boundary diffusion (GBD) effectively enhances the coercivity of Nd–Fe–B sintered magnets, excessive Tb consumption near the magnet surface limits Tb utilization efficiency. We designed Tb (80−x) La x Cu 15 Al 5 (x = 0, 20, 40, and 60) (wt.%) diffusion sources by partially replacing Tb with La to control the GBD behavior and improve Tb utilization efficiency. The effects of La content on the magnetic properties, microstructure, and thermal stability of the GBD magnets were investigated. The La-containing GBD magnets exhibited enhanced Δ H cj /Tb wt.%, suppressed B r reduction, and superior squareness while reducing Tb consumption compared with the Tb 100 -diffused magnet. In particular, the Tb 40 La 40 Cu 15 Al 5 -GBD magnet exhibited higher H cj and ( BH ) max than the Tb 100 -GBD magnet, and its Δ H cj /Tb wt.% increased by 157%. Elemental mapping revealed that La addition suppressed excessive Tb accumulation near the magnet surface by reducing Tb substitution for Pr. Consequently, the formation of a thick Tb-rich shell was suppressed, resulting in a thinner and more continuous Tb-rich shell. In addition, the La-containing GBD magnets exhibited improved thermal stability comparable to those of the Tb 100 - and Tb 80 Cu 15 Al 5 -GBD magnets. These results indicate that partial replacement of Tb with La in the diffusion sources controls near-surface Tb accumulation and Tb-rich shell formation, thereby improving Tb utilization efficiency and the magnetic properties of Nd–Fe–B sintered magnets.
No takes yet. Share an insight, caveat, or question.
Kim et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: