Answers are grounded in this paper and cite their sources.
Tungsten oxide films were deposited on unheated glass substrates by reactive DC magnetron sputtering at a constant total working pressure of 2.8 Pa while systematically varying the oxygen partial pressure. The influence of oxygen partial pressure and the associated discharge response on film growth, crystalline structure, surface morphology, roughness and optical behaviour was investigated. X-ray diffraction showed that the as-deposited films were amorphous or poorly crystallized, whereas annealing in air at 400 °C for 2 h promoted the formation of crystalline WO₃-type structures that could be ascribed to a monoclinic space group. The crystallite size exhibited a pronounced non-monotonic dependence on oxygen partial pressure. SEM and AFM revealed continuous nanostructured granular coatings whose morphology, roughness and thickness changed markedly with deposition conditions. In particular, the film thickness showed a strong non-monotonic evolution, decreasing from approximately 13 µm at 10% O₂ to below 1 µm at 40% O₂, followed by a marked increase at 50–60% O₂. This behaviour indicates substantial changes in the reactive-sputtering and coating-growth conditions. UV–Vis measurements yielded Tauc-derived apparent optical gaps between approximately 1.7 and 2.9 eV. The optical response was found to reflect the combined evolution of film thickness, crystalline structure, surface morphology and roughness. The results reveal a strong coupling between oxygen partial pressure, discharge response, coating growth and the resulting microstructural and optical properties of reactive-sputtered tungsten oxide films.
No takes yet. Share an insight, caveat, or question.
Moura et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: