In this work, the influence of post-treatment on the physical and mechanical properties of AlSi10Mg processed by laser powder bed fusion (L-PBF) on an EOS M 290 machine in three build orientations (0°, 45° and 90°) was analyzed quantitatively. The post-treatments comprised solution treatment (530 °C/2 h, water quenching) followed by natural aging (T4 temper) or by artificial aging at 150, 175 or 200 °C for 2 h (T6 temper), as well as hot isostatic pressing (HIP; 530 °C, 100 MPa, 2 h) and HIP followed by T6 aging at 175 °C (HIP + T6). Density measurements, Vickers hardness (HV0.2) tests, tensile tests, impulse excitation measurements of Young's modulus and fractography were carried out. The as-fabricated (AF) state showed the highest strength (ultimate tensile strength 474–506 MPa, yield strength 237–287 MPa) but the lowest elongation (≈6–10%) and a relative density of 97.6–98.9%. Solution treatment and aging decreased the strength by 35–40% and increased the elongation to ≈12–22%, but did not affect the porosity; aging at 175 °C gave the best T6 properties. HIP increased the relative density to 99.1–99.7% but halved the hardness, whereas HIP + T6 combined a relative density of 99.8–99.96% with ≈75–90% of the AF hardness, a tensile strength of ≈295–325 MPa and an elongation of ≈10–12.5%, and reduced the orientation-related difference in density from 1.24 to 0.14 percentage points. The findings of this comprehensive parametric study indicate that HIP + T6 provides the optimal combination of properties for meeting the mechanical requirements of industrial applications.
No takes yet. Share an insight, caveat, or question.
Ece et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: