Micro-square through-holes were fabricated in 0.8 mm-thick AA6061–10 wt% TiB 2 composite plates using pulsed Nd:YAG laser raster scanning. At a fixed nominal average power of 140 W and a pulse repetition frequency of 4 kHz, scanning speeds of 25, 35, and 45 mm/s corresponded to nominal linear energy inputs of 5.60, 4.00, and 3.11 J/mm, respectively. Hole morphology, surface topography, elemental distribution, and local microstructure were examined using field-emission scanning electron microscopy (FESEM), optical profilometry, energy-dispersive X-ray spectroscopy (EDS), X-ray diffraction (XRD), and transmission electron microscopy (TEM). The 25 mm/s condition exhibited substantial adherent resolidified material and an inner-wall roughness of approximately 0.115 µm. At 45 mm/s, irregular hole boundaries and exposed reinforcement particles were observed, with roughness of approximately 0.128 µm. Among the three conditions examined, 35 mm/s yielded the smallest reported dimensional deviations from the target aperture, with an entrance measuring approximately 253.1 × 250.3 µm and roughness of approximately 0.070 µm. The maximum reported microhardness at this speed was approximately 133 HV, compared with approximately 75 HV in the unaffected composite. The principal Al and TiB 2 phases were observed after machining; weak additional diffraction features were suggested the possible presence of to Al 3 Ti but require confirmation. The results identify 35 mm/s as the most favourable of the tested scanning speeds for entrance geometry and measured surface roughness. The effects of raster geometry, measurement uncertainty, and inferred removal mechanisms require further validation.
No takes yet. Share an insight, caveat, or question.
Raman et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: