Localized wrapping defects may weaken vortex-spun yarn. This study examined the spatial correspondence between image-detected wrapping defects and break locations, and how defect features relate to breaking force. Viscose and polyester vortex-spun yarns (19.68 and 9.84 tex) were imaged online to automatically detect and segment defects. Positional correspondence across 400 paired defect–break records was tested against Monte Carlo randomization. Defects were characterized by aspect ratio, perimeter–area ratio (PAR), angular second moment, inverse difference moment (IDM), and entropy (ENT), then integrated via entropy weighting into a Wrapping Defect Severity Index (WDSI). Correlation and mixed-effects regression showed a median defect-to-break distance of 82.0 mm versus 150.0 mm under randomization (RMD = 0.547), significant in all groups. PAR and ENT correlated negatively with breaking force, while IDM showed the strongest positive association. WDSI had negative linear and quadratic effects across all groups, supporting its use in yarn quality assessment.
No takes yet. Share an insight, caveat, or question.
Jin et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: