In soft–rigid robotics, it is necessary to join flexible polymers to each other and to rigid thermoplastics without using adhesives or fasteners. However, little is known about ultrasonic welding of elastomers. In this study, we examine the 20 kHz ultrasonic welding of fused deposition modelling (FDM)-printed thermoplastic polyurethane (TPU) and its joining to polylactic acid (PLA). Flat interfaces did not weld in any of the 63 pair-thickness conditions tested (n = 5 per pair), with the halves separating at mean peak loads of 5.0–8.0 N. A hexagonal energy director, which was developed for use with rigid polymers, was ineffective. However, an interlocking toothed profile (tooth thickness 0.7–1.0 mm, pitch 1 mm, height 1 mm) was able to weld TPU–TPU with a total thickness of up to 5 mm with 80% amplitude, using a soft vibration ramp and a weld time of 2–3 s (peak load 29.0 ± 1.6 N). The same profile was used to join TPU to PLA. At a total thickness of 5 mm, the joints failed at the weld line (39.0 ± 1.6 N); at 10 mm, four out of five specimens failed in the base material at 62.0 ± 3.4 N. The need for an energy director is attributed to the low stiffness and high damping of TPU. Only macroscopic and optical microscopic examinations were performed; the positioning was manual and only quasi-static loading was tested. Polished sections, fatigue and creep tests are still needed.
No takes yet. Share an insight, caveat, or question.
Chibukhchyan et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: