Investigation demonstrates 99.99% detoxification efficiency in cyanide-laden tailings, indicating sodium percarbonate's viability for eco-friendly remediation.
Cyanide-containing effluents from hydrometallurgical gold extraction pose significant environmental risks due to their high toxicity. This study investigates the detoxification of cyanide-laden tailings from the Altyntau Kokshetau gold extraction facility (Kazakhstan) using sodium percarbonate in alkaline conditions. Employing response surface methodology (RSM) and central composite design (CCD), we optimized key parameters—pH (10–12), sodium percarbonate dosage (1.5–4.0 g), reaction time (10–40 min) and temperature (20–25 °C)—achieving 83.33% detoxification efficiency within 40 min and 99.99% after 8 h, reducing cyanide from 443.2 mg/L to 0.05 mg/L. The process follows biphasic pseudo-first-order kinetics ((k1 = 0.0517) min–1 initially, (k2 = 0.01665) min–1 subsequently), driven by HO• radical-mediated oxidation of CN– to CNO–, as described by (CN– + H2O2 → CNO– + H2O). pH emerged as the dominant factor, optimizing radical stability and CN– protonation (pKa ≈ 9.21) at pH 10. Infrared spectroscopy confirmed the presence of cyanide complexes ([Au(CN)2]–, [Fe(CN)6]4–) in tailings, underscoring the need for effective treatment. The method ensures compliance with stringent environmental standards (e.g., ICMI limit of 0.2 mg/L), offering a scalable, eco-efficient solution for mitigating the environmental footprint of gold mining operations.
No takes yet. Share an insight, caveat, or question.
Berkinbayeva et al. (2025) studied this question.
Synapse has enriched 5 closely related papers on similar clinical questions. Consider them for comparative context: