The selection of fatigue crack growth records influences Paris-law fitting and retrospective cycle estimates. Eight ASTM A572 Grade 50 C(T) datasets were examined under two acquisition histories: MB_01–MB_03 contain a continuous record of fatigue-precrack formation and subsequent propagation, whereas MB_04–MB_08 contain propagation records acquired after separate precracking. The measured machined notch (approximately 12 mm) defines the initial reference for the first group; the measured notch plus the 3 mm programmed precrack extension provides only a nominal post-precrack reference for the second. To compare eligible propagation data, records before the nominal post-precrack length were excluded from the fitting selections of MB_01–MB_03. Laboratory-referenced and fixed minima-based algorithmic selections were evaluated using common geometric limits, regression-start sensitivity, matched retrospective cycle integration, and paired leave-one-specimen-out (LOSO) transfer. The algorithm showed a smaller local variation in exponent m in five specimens, with two ties, whereas laboratory-constrained fitting yielded lower mean absolute retrospective cycle error (1.76% versus 2.13%). Paired LOSO cycle errors remained similar (9.85% versus 9.49%), without evidence of universal superiority. Mathematical segmentation and six further welded datasets provide complementary operational checks, not a unique physical Region-II boundary.
No takes yet. Share an insight, caveat, or question.
Santos et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: