Answers are grounded in this paper and cite their sources.
Additively manufactured Ti–6Al–4V lattice structures are promising candidates for load-bearing biomedical implants, but their fracture and corrosion responses depend on geometry and build orientation. This study examined open-cubic lattices (unit-cell edge, 5.0 mm; strut diameters, 1.0 and 1.5 mm) produced by direct metal laser sintering in horizontal (H) and vertical (V) build orientations, stress relieved at 650 °C and vacuum heat treated at 950 °C for 2 h. Scanning electron microscopy (SEM) fractography showed dimples and tear ridges consistent with ductile failure. Pooled over strut sizes, the compressive moduli were 3.3 ± 0.2 GPa (H) and 2.8 ± 0.2 GPa (V), whereas the yield strength was higher for V builds (78.4 ± 5.0 versus 52.9 ± 4.1 MPa). In 14-day immersion tests in aerated 10 wt% NaCl at 37 °C (three specimens per condition), the H lattices had lower mass-loss corrosion rates than the V lattices (0.063 versus 0.078 mm/year for 1.0 mm struts; 0.091 versus 0.103 mm/year for 1.5 mm struts), but the ranking for the 1.5 mm struts depended on the area normalization, and single polarization curves per condition did not give a consistent orientation ranking; an orientation effect on corrosion is therefore not established. Finite element and extended finite element models identified strut junctions as stress-concentration sites, and a Gutman-type estimate gave a local potential shift of −14.2 mV. These model outputs are qualitative because they were not quantitatively validated, and no mechanical load was applied during corrosion testing.
No takes yet. Share an insight, caveat, or question.
Ochonogor et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: