Laser powder bed fusion (LPBF) Ti–6Al–4V shows orientation-dependent fatigue behavior that tensile properties and bulk density do not fully explain. Vertical (VT) and horizontal (HZ) specimens were annealed at 850 °C for 2 h (furnace cooling) and characterized by optical and scanning electron microscopy, X-ray diffraction (XRD) with Rietveld refinement, micro-computed tomography (micro-CT), Vickers hardness, tensile tests, and high-cycle fatigue tests (R = 0.1). The annealed material consisted of α + β (approximately 88–92 vol.% α and 8–12 vol.% β). Tensile properties of the two orientations were similar, with HZ specimens slightly stronger and of similar elongation. Despite a bulk density above 99.9%, micro-CT revealed isolated pores of roughly 60–270 μm. At 600 MPa, VT specimens failed after 6.79 × 104 and 7.36 × 104 cycles, whereas HZ specimens failed after 8.82 × 105 and 1.37 × 106 cycles. Fatigue data at other stress levels are limited, so the orientation effect is demonstrated only at 600 MPa, where two specimens per orientation were tested. The results indicate that defect size, morphology, and orientation relative to the load, rather than tensile properties or density, are the likely cause of the anisotropy. An orientation-sensitive descriptor, F = dmax cos2θ, is proposed as a hypothesis; specimen-resolved defect data exist for only three VT specimens, so it remains to be validated. No as-built control was tested, and conclusions apply to the annealed condition.
No takes yet. Share an insight, caveat, or question.
Ochonogor et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: