Research investigates meso-scale degradation in thin asphalt overlays, suggesting improvement methods for durability.
Premature skid resistance deterioration is a critical issue limiting the long-term performance of thin asphalt overlays. To elucidate the meso-scale degradation mechanisms, this study employs the Discrete Element Method (DEM) implemented in Particle Flow Code (PFC) to compare a conventional Stone Matrix Asphalt (SMA-10) mixture with an optimized skeleton-reinforced design, termed Optimized Gradation-10. The optimized gradation was developed by introducing supplementary sieve sizes of 5.6, 6.7, and 8.0 mm within the critical range of 4.75–9.5 mm following the V–S gradation framework. Cross-sectional images of actual mixtures were vectorized using Python (Version: 3.11.5) and MATLAB (Version: R2024a) to reconstruct irregular aggregate clump models that accurately capture particle morphology and spatial arrangement. Meso-scale parameters were calibrated and validated through uniaxial compression tests, and the evolution of contact number, contact force, and stress transmission was analyzed under 2.3 × 105 wheel load cycles. Compared with SMA-10, the optimized mixture increased effective aggregate contacts by 41.8%, enhanced stress transfer efficiency by 19.8%, and reduced rut depth by 10%. These findings confirm that synergistic gradation optimization through supplementary sieves and the V–S method markedly improves structural stability and deformation resistance, providing a meso-mechanical foundation for prolonging skid resistance in thin overlays.
No takes yet. Share an insight, caveat, or question.
Rehman et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: