Answers are grounded in this paper and cite their sources.
Experimental work demonstrates improved dielectric properties in ceramics, suggesting lower sintering temperatures can be achieved.
Using solid-state synthesis in the ZrO2–SnO2–TiO2 system with the La2O3 and ZnO sintering additives, dense ceramics with a Q factor of 400, a permittivity of 34, an open porosity of 0.3%, a zirconium–tin titanate crystal size of 5–7 μm, and a closed porosity of up to 3% has been obtained. The Zr0.8Sn0.2TiO4 dielectric has a sintering temperature of 1350°C, which is 200–250°C lower than the value for the commercial analogs.
No takes yet. Share an insight, caveat, or question.
Zolottsev et al. (2026) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: