Answers are grounded in this paper and cite their sources.
InGaPAs-InP double-heterojunction (DH) high-radiance LED's (λ ∼ 1.05-1.3 µm) have been fabricated by liquid-phase epitaxy (LPE) at constant temperature. The crystal growth procedure is described and the influence of InP substrate crystalline perfection is discussed. LED's with a high-radiance geometry suitable for coupling to an optical fiber have been fabricated. The four-layer double-heterostructure LED's have low forward-biased resistances. Typical external quantum efficiencies of ∼1.5 percent and narrow emission linewidths (∼56 nm, typical), have been measured for LED's (λ ∼ 1.08 µm) with an InGaPAs active layer thickness of 1.6 µm and an active layer carrier concentration of <tex xmlns:mml="http://www.w3.org/1998/Math/MathML" xmlns:xlink="http://www.w3.org/1999/xlink">NA - ND ≈ 2.8 \× 10¹⁶</tex> cm -3 . The dependence of LED emission linewidth upon active layer doping is reported. Transient measurements show that the LED rise time is dependent upon current density for high-injection conditions. Preliminary lifetest results demonstrate only slight LED degradation after operation at 50 and 70°C for times up to ∼3500 h.
No takes yet. Share an insight, caveat, or question.
Wright et al. (1979) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: