Answers are grounded in this paper and cite their sources.
High-purity Li single crystals in the b.c.c. phase are deformed in the temperature range between 78 and 400 K in tension and compression. Below T0 = 250 K (= 0.55 Tm) the flow stress shows a strong increase with decreasing temperature, an orientation dependence, and asymmetry in tension and compression. The activation volume has values of several thous and b3. This and other observations rule out formation of kink pairs as rate-controlling process and suggest a forest intersection mechanism. This is corroborated by comparison with TEM observations in the literature.
No takes yet. Share an insight, caveat, or question.
Gorgas et al. (1981) studied this question.