SiCN films were produced by remote microwave hydrogen plasma CVD (RP‐CVD) from tris(dimethylamino)silane precursor using different substrate temperature in the range T S =30‐400°C. The effect of T S on the rate of RP‐CVD, chemical structure, surface morphology, density, and photoluminescence (PL) of resulting films is reported. The increase in T S causes the formation of silicon carbonitride network, marked densification and smoothening of film surface, as well as shift of PL peak position.