Answers are grounded in this paper and cite their sources.
Intermediate valence compound YbAl 3 has been synthesized by the Bridgman method. Temperature dependence of the Seebeck coefficient, electrical resistivity and thermal conductivity has been measured on YbAl 3 hot-pressed and single crystal samples. At temperatures below 100 K, the electrical resistivity exhibits a ρ( T ) = ρ 0 + AT 2 dependence, while over the temperature range 300-800 K YbAl 3 exhibits metallic behaviour with a linear temperature dependence of the electrical resistivity. The Seebeck coefficient exhibits a temperature dependence typical for heavy fermion compounds and attains a maximum of its absolute value of -79 µV K -1 at around 200-250 K. Combination of a large Seebeck coefficient and low residual resistivity of single crystalline YbAl 3 leads to the highest ever reported electrical power factor of 340 × 10 -6 W cm -1 K -2 at 80 K. Thermal conductivity as a function of temperature has a broad peak at 50 K, which originated mainly from the electronic contribution to thermal conductivity. At 300 K the total thermal conductivity of hot-pressed samples ranges from 0.085 to 0.179 W cm -1 K -1 depending on the density of the samples. The calculated figure of merit value attains its maximum of 1 × 10 -3 K -1 at 100-120 K.
No takes yet. Share an insight, caveat, or question.
Rowe et al. (2002) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: