Answers are grounded in this paper and cite their sources.
The resistivity and Hall coefficient RH for Zn-doped GaP were measured at temperatures between 4.2° and 775°K. Neutron activation and through diffusion with radioactive 65Zn were used to determine the Zn concentration NZn, which ranged from 6.7×1016 cm−3 to 2.1×1019 cm−3. At the lowest Zn concentration the thermal ionization energy for Zn in GaP was found to be 0.060±0.002 eV. The thermal ionization energy decreases rapidly for Zn concentrations in excess of 2.0×1017 cm−3. Metallic impurity conduction was observed at a Zn concentration of 2.1×1019 cm−3. The low-concentration region is observed for NZn≲2.0×1017 cm−3, the intermediate-concentration region for 2.0×1017≲NZn≲2.1×1019 cm−3, and the high-concentration region for NZn≳2.1×1019 cm−3. In the intermediate-concentration region the high-temperature hole concentration, determined from p=1/eRH, was found to exceed the Zn concentration by a significant amount. Analysis of the temperature-dependent hole concentration results in an effective density-of-states mass ratio of approximately 0.5. The lightest doped sample had a room-temperature Hall mobility of 120 cm2/V·sec and a maximum mobility of 2050 cm2/V·sec at 55°K. The maximum mobility at low temperature is limited by ionized and neutral impurity scattering, while the dominant high-temperature scattering mechanism appears to be optical phonon scattering.
No takes yet. Share an insight, caveat, or question.
Casey et al. (1969) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: