Answers are grounded in this paper and cite their sources.
Optical waveguides consisting of a pure fused silica core and borosilicate cladding were produced by using chemical vapor deposition techniques. A typical guide showed an optical attenuation of 7.5 ± 1.5 dB/km, measured at 0.63 μm (He–Ne laser). In one of the guides whose loss spectrum was studied, the attenuation was less than 20 dB/km between 0.55 and 0.86 μm except for the third OH overtone at ∼ 0.72 μm. The lowest loss of this waveguide occurred at 0.80 μm, with other minima at 0.66 and 1.06 μm.
No takes yet. Share an insight, caveat, or question.
French et al. (1973) studied this question.