Preoxidation of Ti 3 AlC 2 at 1100°C for 2 h was conducted to improve its cyclic‐oxidation resistance at the testing temperature of 550°C and 650°C in air. The cyclic oxidation of the preoxidized Ti 3 AlC 2 was found to follow a parabolic rate law rather than the linear oxidation rate for that without preoxidation. Through the X‐ray diffraction and SEM analysis, the remarkable improvement of the cyclic‐oxidation resistance of preoxidation Ti 3 AlC 2 is suggested due to the existence of protective α‐Al 2 O 3 layers formed during the preoxidation treatment, which inhibits the formation of amorphous Al 2 O 3 , which can result in larger thermal stress and stress‐induced microcracks.