We measured the size- and shape-dependent compressibility of the TiO 2 anatase nanoparticles using monochromatic synchrotron X-ray powder diffraction and high-pressure diamond-anvil cell techniques. Compared to the bulk anatase sample, the rice-shaped (3.8 × 5.0 nm) and the rod-shaped (3.5 × 21.0 nm) anatase nanoparticles exhibit reduced and enhanced bulk modulus, respectively, ranging between 204(8) and 319(20) GPa. The Williamson−Hall plot analysis of the measured diffraction data from the bulk sample shows that the pressure-dependent increase of the microscopic strain is isotropic, whereas the Strokes−Wilson profile analyses on the two resolved Bragg peaks from the anatase nanoparticles reveal anisotropic distribution and evolution of the relative strain. This might be attributed to the higher c -axial compressibility and also to the higher population contrast of the hard TiO 6 and soft O 6 octahedra in the nanoparticle samples compared to the bulk sample.
No takes yet. Share an insight, caveat, or question.
Park et al. (2008) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: