Answers are grounded in this paper and cite their sources.
The formation of the recoil impulse of the laser ablation products of polystyrene and its composite with carbon nanotubes (CNTs) has been studied. The possibility of using low doses of preliminary γ-irradiation (40–70 kGy) of styrene to obtain stable CNT dispersions in it is shown. Due to an increase in the viscosity of radiolyzed styrene as a result of partial oligomerization, the sedimentation time of the CNT dispersion in it increases many times, thereby making it possible to obtain solid homogeneous dispersions for the manufacture of laser ablation targets by subsequent additional γ-irradiation. The average ablation rate for the individual polymer at a laser radiation power of 40–45 W is 10.3 mg/s, and it linearly decreases in proportion to the amount of CNTs introduced into the polystyrene matrix. Thus, nonmonotonic relationships of the specific and the maximum recoil impulse versus the CNT content in the composite are observed, having minima at Csp = 4.01 ± 0.05 μN·s/J and Cm = 38.66 ± 0.10 μN s, respectively, in the case of ablation of the composite containing 0.04 ± 0.10 wt % CNT. The specific recoil impulse of the products of laser ablation of targets made of individual polystyrene (5.8 μN/J) and its composite with CNTs (7.6 μN/J) depend in different manners on the dose of their preliminary γ-irradiation. In contrast to the case of composite, for which the recoil impulse decreases with the dose of its preliminary radiolysis, this impulse in the ablation of radiolyzed polystyrene increases with the γ-treatment dose.
No takes yet. Share an insight, caveat, or question.
Frolov et al. (2022) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: