Answers are grounded in this paper and cite their sources.
Indexed powder patterns are reported for three homogeneous metastable ZrO 2 -CeO 2 solid solution members with high-zirconia [(ZrO 2 ) x mole fraction, x>.84 –.80] and lowzirconia (.60>x>.40) compositions. The primitive cell dimensions are: a = 3.6377(7) Å and c = 5.2394(11) Å at x = 0.84, and a = 3.7205(5) Å and c = 5.3039(7) Å at x = 0.5. Samples with intermediate compositions are heterogeneous. Also reported are powder data for the cubic (fluorite-structure) solution from a sample with x = 0.40 and a slightly different thermal history.
No takes yet. Share an insight, caveat, or question.
Meriani et al. (1987) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: