To develop catalysts with superior stability for isobutane alkylation, La 3+ exchanged FAU zeolites with varying framework Si/Al ratios were investigated. Based on the reaction performed in a continuous flow stirred tank reactor, a strong linear relationship between catalyst lifetime and strong Brønsted acid concentration was observed. Catalyst lifetime was speculated to change in an M-shaped pattern with respect to the framework Si/Al ratio, which implies there were at least two extreme Si/Al ratios in terms of catalyst stability. However, their product distribution differed significantly. LaFAU with a high Si/Al ratio led to enhanced acid strength, which resulted in higher cracking, self-alkylation activity, and poor product selectivity. In determining a balance between catalyst stability and product selectivity, a Si/Al ratio of ∼1.2 was selected as the optimal value for LaFAU zeolites.
No takes yet. Share an insight, caveat, or question.
Yang et al. (2020) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: