Ultrametastable silicon-germanium (Si1−xGex) layers with a Ge content x in the range from about 20% to 27% were grown by Si-MBE at temperatures far below 550 °C (325–450 °C). The thicknesses of the layers (up to 500 nm) exceed the equilibrium thickness by a factor of up to 50. We observe in the as-grown samples without any annealing both the excitonic Si1−xGex band-edge luminescence and a broad alloy luminescence of unknown origin. The two peaks have an energy difference of ≊144 meV and shift linearly with the Ge content. The alloy band luminescence disappears when strain relaxation sets on upon annealing at around 600 °C.