Al2O3 synthesized by atomic layer deposition (ALD) on H-terminated Si(100) exhibits a very thin (∼1 nm) interfacial SiOx layer. At this interface, a high fixed negative charge density, Qf, is present after annealing which contributes to ultralow surface recombination velocities <2 cm/s. Here, we identify the thickness of the interfacial SiO2 layer as a key parameter determining Qf. The SiO2 thickness was controlled by intentionally growing ultrathin SiO2 interlayers (0.7−30 nm) by ALD. Optical second-harmonic generation spectroscopy revealed a marked decrease in Qf for increasing SiO2 thickness between 0 and 5 nm. This phenomenon is consistent with charge injection across the interfacial layer during annealing. For thicker SiO2 interlayers (>∼5 nm), the polarity of the effective charge density changed from negative to positive. The observed changes in Qf and the associated field-effect passivation had a significant influence on the injection-level-dependent minority carrier lifetime of Si.
No takes yet. Share an insight, caveat, or question.
Dingemans et al. (2011) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: