Group V impurities implanted at 400 keV into silicon have been detected in substitutional lattice positions by EPR. Three samples of VFZ, p-type 1200–1500 ohm-cm silicon from the same ingot were implanted with As75, Sb121, and Sb123, respectively. The EPR spectrum of each implanted substitutional impurity was observed after annealing the lattice damage. Only the isotope implanted in each sample was seen. Since only those donors which are electrically active can be observed, this technique measures the electrically active fraction of the implanted species. Upon annealing to 970°C, most of the antimony was active whereas only about 1/5 of the arsenic was observed. Comparisons with backscattering results indicate that between 350 and 600°C, ∼95 per cent of the implanted antimony is substitutional but ∼0 per cent is electrically active. The increase in electrical activity at 600°C is due to the rise of the Fermi level to the donor level as the residual lattice damage anneals. The paramagnetic damage centers observed were those also seen in oxygen-implanted silicon, Si-P3 and Si-Pl, but the Si-P3 center was not as well resolved and grows upon annealing to 200°C.
No takes yet. Share an insight, caveat, or question.
Borders et al. (1970) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: