Answers are grounded in this paper and cite their sources.
We have activated epitaxial layers of vapor-deposited Ga1−xInxAs alloys in the bandgap range 0.96–1.18 eV with Cs and O2. The Cs–O was determined to be ∼1 monolayer thick. For each sample the photothreshold energy was approximately equal to the bandgap energy. A long-wavelength limit of approximately 1.3 μm was determined for valence-band emission. There was no evidence of an internal barrier which might have decreased this limit. Spectral yield data were analyzed to give a surface escape probability versus bandgap plot.
No takes yet. Share an insight, caveat, or question.
Fisher et al. (1971) studied this question.