Minority-carrier recombination lifetime mapping has been performed with a noncontact laser/microwave photoconductance method for as-polished wafers containing a ring-shaped distribution of embryonic defects which form stacking faults during subsequent heat treatment. Using an algorithm for the separation of bulk and surface components of the recombination lifetime, four regions, which cannot be distinguished with other techniques such as x-ray topography and preferential chemical etching, were clearly observed in the maps as those with different lifetimes. The result can be attributed to the inhomogeneous distribution of grown-in defects, most likely intrinsic point defects and/or oxygen related defects. Moreover, the lifetime was correlated to the surface microroughness of the polished wafers.