Two types of low-temperature Au–Si wafer bonding structure (i.e. Au/Si and Au/Au bonding structures) were investigated in this paper. The bond quality test showed that bond yield, bond repeatability and average shear strength are lower for the Au/Si bonding structure. The interfacial microstructure analysis of the Au/Si bonding structure suggested that the craters at the bonding interface are due to the anisotropy and non-uniformity of the Au/Si reaction, and the non-uniformity of the Au/Si reaction results in poor bond quality. The anisotropy of the Au/Si reaction is mainly because of the difference in the surface energy of each plane of the crystalline Si, and the non-uniformity of the Au/Si reaction is due to the native oxide on the bare Si surface. In the Au/Au bonding structure, a Ti/Au layer is deposited onto the bare Si surface, in which the Ti layer is used to decompose the native oxide during bonding. With this bonding structure, the bond yield, bond repeatability and average shear strength have improved significantly compared to the Au/Si bonding structure. The interfacial microstructure analysis indicated that the native oxide on the Si surface is decomposed by Ti during bonding, thereby causing the Si dissolution into Au to occur uniformly over the whole bonding interface and achieving a good bond quality. Remarkably, the measured thickness of the bonding interface has increased compared to that of the as-deposited metallic film, which is primarily attributed to the fact that Si from the substrate dissolves into the Au uniformly and then the Si precipitate forms across the bonding interface.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Jing et al. (2010) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: