Silicon specimens have been irradiated at temperatures up to 650°C, and the resultant structures examined in detail. The principal defect is an extrinsic {113} fault, elongated in ⟨110⟩, with a displacement close to a/11⟨113⟩. Below 500°C these defects may change plane, along their long axes, such that the angle between faces is obtuse. Between 500°C and 600°C isolated {113} faults may unfault, to form interstitial loops on {113}, elongated in ⟨110⟩, with b = a/2⟨1. At 650°C, complex unfaulting, involving two intersecting {113} faults, may occur. Nickel-implanted silicon was found to contain a variety of unfaulted and complex defects after annealing at 800°C. No evidence of interstitial aggregation to form a/3⟨111⟩ faults on {111} was found, and it is suggested that {111} precipitates require the presence of oxygen. The tetrahedral model for the {113} fault is developed, and it is shown that this may account for all defects found in irradiated silicon and germanium, and in implanted silicon after annealing in an inert (i.e. oxygen-free) environment.
No takes yet. Share an insight, caveat, or question.
Salisbury et al. (1981) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: