We report an effective approach to reduce defects at a SiC/SiO2 interface. Since oxidation of SiC may inevitably lead to defect creation, the idea is to form the interface without oxidizing SiC. Our method consists of four steps: (i) H2 etching of SiC, (ii) Si deposition, (iii) low-temperature (∼750 °C) oxidation of Si to form SiO2, and (iv) high-temperature (∼1600 °C) N2 annealing to introduce nitrogen atoms. The interface state density estimated by a high (1 MHz)–low method is in the order of 1010 cm−2 eV−1, two orders of magnitude lower than that of an interface formed by SiC oxidation.