Answers are grounded in this paper and cite their sources.
Mechanical property and corrosion resistance of TIG welded UNS S32760 super duplex stainless steel were studied in the present work. The sample surfaces were peened using bigger steel balls with higher intensity followed by another two stages of peening using smaller steel/glass balls at a lower intensity. Six different multiple shot peening parameters were applied onto the weld bead identified by SP1 through SP6. The microstructure and mechanical property of the weld bead was assessed through surface morphology, surface roughness, residual stress measurement, X-ray diffraction. Potentiodynamic polarization studies were carried out in 3.5% NaCl solution to understand the corrosion behavior. In general, it was found that the use of glass beads in the last stage of shot peening resulted in superior mechanical properties and corrosion resistance compared to peening using steel balls in all the three stages. Among the different treatments, SP2 parameter demonstrated superior microhardness (381.4 HV) and high residual stress (-880 MPa and -986.8 MPa in ferrite and austenite phase, respectively). Relatively higher domain size and lower microstrain along with low surface roughness of 1.25 µm (Ra) was responsible for the lowest corrosion rate (0.021mpy) in the SP2 treated weld bead.
No takes yet. Share an insight, caveat, or question.
Vishwanatha et al. (2025) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: