An epitaxial TiO 2 -anatase thin film was grown on the Si(001) substrate with SrTiO 3 /TiN as the buffer layers by the pulsed laser deposition technique under an oxygen gas supply. The typical thicknesses of TiO 2 -anatase, SrTiO 3 and TiN layers were 760 nm, 450 nm and 230 nm, respectively. The characterization of the epitaxial TiO 2 -anatase film was performed using the x-ray diffraction method. The crystallographic relationships between the TiO 2 -anatase film and SrTiO 3 /TiN buffer layers were analysed by the θ-2θ scan and pole figure measurement. The growth direction of the films was determined as TiO 2 ⟨001⟩/SrTiO 3 ⟨001⟩/TiN⟨001⟩/Si⟨001⟩ and their in-plane relationship TiO 2 {110}||SrTiO 3 {100}||TiN{100}||Si{100}. The crystalline quality of TiO 2 -anatase was examined by the rocking curve analysis. The composition of the thin film packaging was characterized by Rutherford backscattering spectrometry (RBS) using a 2.0 MeV 4 He beam. The simulation of the RBS data points to the possible intermixing of Ti (from TiN) and Si.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
Sugiharto et al. (2001) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: