The morphological effect of Al 2 O 3 on the deactivation of V 2 O 5 /Al 2 O 3 catalyst by SO 2 for the removal of NO with NH 3 has been examined to identify the promise of alumina as a support for commercial SCR catalysts. A test program for accelerated batch-type deactivation at 400 °C and accelerated continuous deactivation at 250 °C was developed for V 2 O 5 /Al 2 O 3 catalysts containing distinctive pore size distributions of Al 2 O 3 . The pore size of the catalyst was critical for the deactivation of V 2 O 5 /Al 2 O 3 catalyst along with the surface area. A catalyst containing a high surface area with large mean pores might be an ideal catalyst exhibiting a prolonged catalyst lifetime prolonged for the SCR process because of the SO 2 . The content of vanadia on the surface of Al 2 O 3 is also important in elucidating the role of the morphology of the support in the deactivation of the catalyst. For the batch deactivation test of the catalyst at 400 °C, a high vanadia content of about 20 wt % is required on the catalyst surface, whereas a low content of 7 wt % is appropriate for continuous deactivation at 250 °C. V 2 O 5 /Al 2 O 3 catalysts at 250 °C are easily deactivated by pore filling and/or pore plugging resulting from the formation of deactivating agents such as NH 4 HSO 4 and (NH 4 ) 2 SO 4 . At 400 °C, Al 2 (SO 4 ) 3 and AlNH 4 (SO 4 ) 2 are generated and slowly plug the pores in the catalyst surface, so that the deactivation is hardly distinctive from that occurring at 250 °C.
No takes yet. Share an insight, caveat, or question.
Soh et al. (2003) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: