The triple-dielectric polysilicon-blocking oxide-silicon nitride-tunnel oxide-silicon (SONOS) structure is an attractive candidate for high density E/sup 2/PROMs suitable for semiconductor disks and as a replacement for high-density dynamic random access memories (DRAMs). Low programming voltages (5 V) and high endurance (greater than 10/sup 7/ cycles) are possible in this multidielectric technology as the intermediate Si/sub 3/N/sub 4/ layer is scaled to thicknesses of 50 /spl Aring/. The thin gate insulator and low programming voltage enable the scaling of the basic memory cell and associated complementary metal-oxide-semiconductor (CMOS) peripheral circuitry on the memory chip. A SONOS 1TC memory cell is proposed in a NOR architecture with a cell area of 6F/sup 2/ where F is the technology feature size. A 0.20 /spl mu/m feature size permits a 1TC area of 0.24 /spl mu/m/sup 2/ for advanced 1-Gb nonvolatile semiconductor memory chips. A physical model is presented to characterize the erase/write, retention and endurance properties of the nonvolatile semiconductor memory (NVSM) SONOS device.
Answers are grounded in this paper and cite their sources.
No takes yet. Share an insight, caveat, or question.
White et al. (1997) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: