The photoluminescence of erbium-doped semi-insulating polycrystalline and amorphous silicon containing 30 at. % oxygen is studied. The films were deposited on single-crystal Si substrates by chemical vapor deposition, implanted with 500 keV Er to fluences ranging from 0.05 to 6×1015 ions/cm2, and annealed at 300–1000 °C. Upon optical pumping near 500 nm, the samples show room-temperature luminescence around 1.54 μm due to intra-4f transitions in Er3+, excited by photogenerated carriers. The strongest luminescence is obtained after 400 °C annealing. Two classes of Er3+ can be distinguished, characterized by luminescence lifetimes of 170 and 800 μs. The classes are attributed to Er3+ in Si-rich and in O-rich environments. Photoluminescence excitation spectroscopy on a sample with 1×1015 Er/cm2 shows that ∼2% of the implanted Er is optically active. No quenching of the Er luminescence efficiency is observed between 77 K and room temperature in this Si-based semiconductor. The internal quantum efficiency for the excitation of Er3+ via photogenerated carriers is 10−3 at room temperature. A model is presented which explains the luminescence data in terms of trapping of electrical carriers at localized Er-related defects, and subsequent energy transfer to Er3+ ions, which can then decay by emission of 1.5 μm photons.
No takes yet. Share an insight, caveat, or question.
Hoven et al. (1995) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: