Vapor‐grown doped with radioactive Zn 65 and Se 75 has been prepared by a halogen transport method. The dopant concentration in the crystals ranged from the mid 10 15 to mid 10 19 atoms/cm 3 . By means of radiotracer and electrical measurements, it was found that the degree of incorporation of the dopant into the growing crystal is dependent on the substrate orientation. Zinc was incorporated into (111)A face growths more readily than into (111)B face growths by a factor of from 12‐ to 25‐fold, depending on zinc concentration in the vapor. Selenium was incorporated into (111)B face growths more readily than into (111)A face growths by a factor of from 4‐ to 35‐fold. Growths on (100) or (110) substrates accepted zinc or selenium dopants to about the same extent as the preferentially doped polar [(111)A or (111)B] face. It was found that selenium had a limit of solubility in an electrically active form of about . The solubility limit for zinc was not reached at 10 19 cm −3 . Studies were also made of undoped and selenium doped growths on higher index orientations. A model is presented to account for the observed orientation effect based on the properties of the (111) double layer.
No takes yet. Share an insight, caveat, or question.
R. C. Taylor (1969) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: