Answers are grounded in this paper and cite their sources.
Very adhesive poly (3‐methyl‐thiophene) and poly (3,4‐dimethyl‐thiophene) films were photoelectrochemically grown on platinum‐plated electrodes. The stability of poly (3‐methyl‐thiophene)‐coated photoanodes is dependent on the nature of the counterion used during the synthesis of the polymer. Best results were obtained with . No film peeling was observed after a 17 h run in a aqueous solution under 30 mW/cm 2 tungsten lamp illumination. This is attributed to the greater density and smaller porosity of the polymer grown with this counterion. However, corrosion of the photoanode occurred, because of the reduction of the polymer to its neutral form where its conductivity is drastically lowered. Reduction of the polymer film was also observed with poly(3,4‐dimethyl‐thiophene), but a comparison between the absorption spectra of electrochemically and chemically reduced polymers suggests that the electrochemical reduction is not complete. This can account for the lack of photocorrosion of after a 4 h run in a electrolyte. The use of more oxidizing redox couples prevented the reduction of the polymer film, but led to a rapid photodissolution of the electrode.
No takes yet. Share an insight, caveat, or question.
Horowitz et al. (1984) studied this question.
Synapse has enriched 10 related papers. Consider them for comparative context: